Improving Mechanical and Corrosion Properties of 6061 Al Alloys via Differential Speed Rolling and Plasma Electrolytic Oxidation.

Materials 2024 March 9
This study explores the combined potential of severe plastic deformation (SPD) via differential speed rolling (DSR) and plasma electrolytic oxidation (PEO) to enhance the material performance of 6061 Al alloys. To this end, DSR was carried out at a roll-speed-ratio of 1:4 to obtain ~75% total thickness reduction and a final microstructure of <1 µm. The rest of the samples were annealed to obtain various grain sizes of ~1, ~25, and ~55 μm. Through DSR, the hardness of the material increased from ~64 to ~102 HV. Different grain sizes altered the plasma behavior which further influence the growth of the coating layer, where the fine grain size produced a compact structure beneficial for corrosion protection. This synergy offers tailored materials ideal for high-performance applications across diverse industries, combining enhanced bulk properties from DSR with optimized surface attributes from PEO.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app