Evaluation of Microstructure and Abrasive Wear-Resistance of Medium Alloy SiMo Ductile Cast Iron.

Materials 2024 March 7
Medium-alloy ductile iron with a SiMo ferritic matrix has very good heat resistance. The addition of chromium and aluminum also increases this resistance. This article presents the impact of chromium and aluminum on the structure of SiMo cast iron, especially their impact on the deformation of the spherical graphite precipitates and the formation of M6 C and M3 C2 carbide phases. These carbides are formed in a ferritic matrix or at the grain boundaries, resulting in increased hardness and a drastic reduction in impact strength. The article presents the influence of heat treatment on the material's microstructure and resistance to abrasive wear. Chromium and aluminum additions can also indirectly reduce the abrasive wear resistance of SiMo cast iron. The presented research shows the possibility of doubling the abrasive wear resistance of SiMo cast iron.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app