Direct Growth of Al2O3 on Black Phosphorus by Plasma-Enhanced Atomic Layer Deposition.
Nanoscale Research Letters 2017 December
Growing high-quality and uniform dielectric on black phosphorus is challenging since it is easy to react with O2 or H2O in ambient. In this work, we have directly grown Al2O3 on BP using plasma-enhanced atomic layer deposition (PEALD). The surface roughness of BP with covered Al2O3 film can reduce significantly, which is due to the removal of oxidized bubble in BP surface by oxygen plasma. It was also found there is an interfacial layer of PO x in between amorphous Al2O3 film and crystallized BP, which is verified by both X-ray photoelectron spectroscopy (XPS) and transmission electron microscopy (TEM) measurements. By increasing temperature, the PO x can be converted into fully oxidized P2O5.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app