Modulated electrochemical oxygen evolution catalyzed by MoS<sub>2</sub> nanoflakes from atomic layer deposition (ALD).
Nanotechnology 2018 November 8
Electrochemical water splitting into H2 and O2 has attracted wide attentions owing to the urgent need for clean and renewable energy sources. However, the scarcity and high-cost limit the large-scale application of noble metal catalysts such as IrO2 and RuO2. In this work, as a low-cost catalyst for the electrochemical O2 evolution reaction (OER), MoS2 nanoflakes were obtained by atomic layer deposition (ALD) using MoCl5 and H2S on carbon fiber paper (CFP) surface. According to the results of electrochemical measurements, the MoS2 nanoflakes exhibit an excellent catalytic activity, and the activity can be modulated by controlling the density and the internal resistance of MoS2 nanoflakes. Moreover, the plasma treatment can further improve the activity of MoS2 nanoflakes, and the reason was discussed through the measurements of contact angle, electrochemical impedance spectroscopy (EIS), and electrochemically active surface area (ECSA). The MoS2 nanoflakes obtained by ALD possess huge values for electrochemical OER as a catalyst.
Full text links
Related Resources
Trending Papers
Heart failure with preserved ejection fraction: diagnosis, risk assessment, and treatment.Clinical Research in Cardiology : Official Journal of the German Cardiac Society 2024 April 12
Proximal versus distal diuretics in congestive heart failure.Nephrology, Dialysis, Transplantation 2024 Februrary 30
Efficacy and safety of pharmacotherapy in chronic insomnia: A review of clinical guidelines and case reports.Mental Health Clinician 2023 October
World Health Organization and International Consensus Classification of eosinophilic disorders: 2024 update on diagnosis, risk stratification, and management.American Journal of Hematology 2024 March 30
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app