Atomic Layer Deposition of Metal Oxide on Nanocellulose for Enabling Microscopic Characterization of Polymer Nanocomposites.
Small 2018 October 17
Analysis of cellulose nanocrystals (CNCs) at low volume fractions in polymer nanocomposites through conventional electron microscopy still remains a challenge due to insufficient contrast between CNCs and organic polymer matrices. Herein, a methodology for enhancing the contrast of CNC, through atomic layer deposition (ALD) of alumina (Al2 O3 ) on CNCs is demonstrated. The metal oxide coated CNC allows clear visualization by transmission electron microscopy, when they are dispersed in water and polyol. A coating of about 6 ± 1 nm thick alumina layer on the CNC is achieved after 50 ALD cycles. This also enables the characterization of CNC dispersion/orientation (at 0.2 wt% loading) in an amorphous cellular system rigid polyurethane foam (RPUF), using backscattered electron microscopy with energy-dispersive X-ray spectroscopy. Microscopic analysis of the RPUF with alumina-coated CNC confirms that the predominant alignment of CNC occurs in a direction parallel to the foam rise.
Full text links
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app