We have located links that may give you full text access.
Microstructure, mechanical properties, biocompatibility, and in vitro corrosion and degradation behavior of a new Zn-5Ge alloy for biodegradable implant materials.
Acta Biomaterialia 2018 October 12
Zinc (Zn)-based alloys are considered a new class of biodegradable implant materials due to their superior chemical stability and processability compared to biodegradable magnesium (Mg) alloys. In this study, we report a new biodegradable Zn-5Ge alloy with highly desirable mechanical, corrosion, and biological properties. Microstructural characterization revealed the effective grain-refining effect of germanium (Ge) on the Zn alloy. Tensile test results indicated that the hot-rolled Zn-5Ge alloy showed an ultimate tensile strength of 237.0 MPa, a yield strength of 175.1 MPa, and an elongation of 21.6%; while as-cast pure Zn showed an ultimate tensile strength of 33.6 MPa, a yield strength of 29.3 MPa, and an elongation of 1.2%. The corrosion rates measured by potentiodynamic polarization tests in Hank's solution in ascending order are: as-cast Zn-5Ge (0.1272 mm/y) < as-cast pure Zn (0.1567 mm/y) < hot-rolled Zn-5Ge (0.2255 mm/y) < hot-rolled pure Zn (0.3057 mm/y). Immersion tests revealed that the degradation rate of as-cast Zn-5Ge is 0.042 mm/y, less than half of that of hot-rolled pure Zn and ∼62% of that of as-cast pure Zn. Moreover, the Zn-5Ge alloy showed excellent in vitro hemocompatibility and the addition of 5% Ge effectively enhanced the hemocompatibility of pure Zn. CCK-8 assay using murine preosteoblast MC3T3-E1 cells indicated that the diluted extracts at a concentration <12.5% of both the as-cast Zn-5Ge alloy and pure Zn showed grade 0 cytotoxicity; the diluted extracts at the concentrations of 50% and 25% of Zn-5Ge alloy showed a significantly higher cell viability than those of pure Zn. STATEMENT OF SIGNIFICANCE: Zinc (Zn)-based alloys are currently considered a new class of biodegradable implant materials due to their excellent processability. Here, we report a novel Zn-5Ge alloy with highly desirable mechanical, corrosion and biological properties. The tensile test results indicated that the hot-rolled Zn-5Ge alloy showed an ultimate tensile strength of 237.0 MPa, a yield strength of 175.1 MPa and an elongation of 21.6%; while as-cast pure Zn showed an ultimate tensile strength of 33.6 MPa, a yield strength of 29.3 MPa and an elongation of 1.2%. The corrosion rate measured by potentiodynamic polarization tests in Hank's solution in the ascending order is: as-cast Zn-5Ge (0.1272 mm/y) < as-cast pure Zn (0.1567 mm/y) < hot-rolled Zn-5Ge (0.2255 mm/y) < hot-rolled pure Zn (0.3057 mm/y). Immersion tests revealed that the degradation rate of the as-cast Zn-5Ge is 0.042 mm/y, less than half of that of the hot-rolled pure Zn, ∼62% of that of as-cast pure Zn. Moreover, the Zn-5Ge alloy showed excellent in vitro biocompatibility.
Full text links
Related Resources
Trending Papers
Challenges in Septic Shock: From New Hemodynamics to Blood Purification Therapies.Journal of Personalized Medicine 2024 Februrary 4
Molecular Targets of Novel Therapeutics for Diabetic Kidney Disease: A New Era of Nephroprotection.International Journal of Molecular Sciences 2024 April 4
The 'Ten Commandments' for the 2023 European Society of Cardiology guidelines for the management of endocarditis.European Heart Journal 2024 April 18
A Guide to the Use of Vasopressors and Inotropes for Patients in Shock.Journal of Intensive Care Medicine 2024 April 14
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app