Random spectrum fatigue performance of severely plastically deformed titanium for implant dentistry applications.
Severe plastic deformation (SPD) has long been known to confer superior mechanical properties for many metals and alloys. In the general field of biomedical devices, and dental implants in particular, the superior strength of SPD-processed commercially pure (CP) titanium, that may surpass that of the stronger Ti6Al4V alloy, has been associated with a superior fatigue resistance. Such a property would make those materials both biocompatible and strong alternatives to the currently used titanium alloy. However, the fatigue characterization reported so far in the literature relies on a very small sample size, thereby precluding any meaningful statistical analysis. This paper reports and compares systematic fatigue testing of various grades as-received and SPD processed Grade 4 CP-Ti using the recently developed random spectrum loading approach, in both air and 0.9% saline solution. The results of this study do not support the claim that the SPD process, albeit causing noticeable strengthening, confers any advantage to Grade 4 CP-Ti in terms of fatigue response.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app