Fabrication of blue-fluorescent nanodiamonds modified with alkyl isocyanate for cellular bioimaging.

This paper describes the fabrication of water-dispersible nanodiamond (ND) clusters with blue fluorescence for cellular bioimaging. Poly(ethylene glycol) carboxyl methyl acid (mPEG-COOH) and alkyl isocyanates with different chain lengths were conjugated onto the surface of the ND clusters for water dispersibility and fluorescence via carbodiimide chemistry. The relative fluorescence intensity was increased with the increases in the chain length of alkyl isocyanate and also their conjugated concentration. The ND clusters (average size of 37.6 nm and zeta potential of 26.6 mV) with mPEG-COOH and octadecyl isocyanate (ODI) emitted relatively higher blue fluorescence intensity under excitation at 350 nm as well as favorable water dispersibility. After cellular uptake of the ND clusters, blue fluorescence inside the cells was confirmed by confocal laser scanning microscopy. The ND clusters conjugated with mPEG-COOH and ODI can potentially be used for cellular bioimaging.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app