Evaluation of the flexural mechanical properties of various thermoplastic denture base polymers.

This study evaluated the flexural mechanical properties of various thermoplastic denture base polymers (six polyamides, four acrylic resins, polyester, polypropylene, and polycarbonate) by three different testing conditions; specimens were tested in water bath at 37°C (Wet/Water, by ISO 20795-1), or in ambient air (Wet/Air) after being immersed in distilled water for 50 h, or after desiccation for 7 days (Dry/Air). The mean ultimate flexural strength (UFS) and flexural modulus (FM) for most products ranged from 27 to 61 MPa and from 611 to 1,783 MPa respectively, which failed to meet the minimum requirements of the international standard, except for polycarbonate (89 and 2,245 MPa). The mean UFS and FM values were ranked Dry/Air>Wet/Air>Wet/Water (p<0.05). In conclusion, the flexural mechanical properties of denture base polymers varied with the products and were significantly affected by the testing medium (air or water) and specimen conditions (wet or dry).

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app