Depth dependant element analysis of PbMg<sub>1/3</sub>Nb<sub>2/3</sub>O<sub>3</sub> using muonic X-rays.
The relaxor PbMg<sub>1/3</sub>Nb<sub>2/3</sub>O<sub>3</sub> (PMN) has received attention due to its potential applications as a piezoelectric when doped with PbTiO<sub>3</sub> (PT). Previous results have found that there are two phases existing in the system, one linked to the near-surface regions of the sample, the other in the bulk. However, the exact origin of these two phases is unclear. In this paper, depth dependant analysis results from negative muon implantation experiments are presented. It is shown that the Pb content is constant throughout all depths probed in the sample, but the Mg and Nb content changes in the near-surface region below 100μm. At a implantation depth of 60μm, it is found that there is a 25% increase in Mg content, with a simultaneous 5% decrease in Nb content in order to maintain charge neutrality. These results show that the previously observed skin effects in PMN are due to a change in concentration and unit cell.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app