Effect of CaCN 2 on the preparation of CaAlSiN 3 :Eu 2+ phosphors.
Highly efficient red-emitting phosphors, CaAlSiN3 :Eu2+ , were successfully prepared by the solid-state method using calcium cyanide (CaCN2 ) as the single calcium source. The influences of crystallization temperature, crystallization time, calcination mode and compounds ratio on the photoluminescent properties were investigated. The CaAlSiN3 :Eu2+ phosphors were obtained with 1 mol% CaCN2 by a two-step calcination procedure at 900°C for 2 h and subsequently at 1600°C for 8 h. The CaAlSiN3 :Eu2+ phosphors showed the strongest luminescent intensity at 660 nm when excited by 468 nm. With an increase in crystallization time, the maximum wavelength of the emission was shifted from 644 nm to 660 nm.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app