Au-Capped GaAs Nanopillar Arrays Fabricated by Metal-Assisted Chemical Etching.

GaAs nanopillar arrays were successfully fabricated by metal-assisted chemical etching using Au nanodot arrays. The nanodot arrays were formed on substrates by vacuum deposition through a porous alumina mask with an ordered array of openings. By using an etchant with a high acid concentration and low oxidant concentration at a relatively low temperature, the area surrounding the Au/GaAs interface could be etched selectively. Under the optimum conditions, Au-capped GaAs nanopillar arrays were formed with an ordered periodicity of 100 nm and pillar heights of 50 nm.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app