Formation of BiFeO 3 from a Binary Oxide Superlattice Grown by Atomic Layer Deposition.
We report on the growth of polycrystalline BiFeO3 thin films on SiO2 /Si(001) and Pt(111) substrates by atomic layer deposition using the precursors ferrocene, triphenyl-bismuth, and ozone. By growing alternating layers of Fe2 O3 and Bi2 O3 , we employ a superlattice approach and demonstrate an efficient control of the cation stoichiometry. The superlattice decay and the resulting formation of polycrystalline BiFeO3 films are studied by in situ X-ray diffraction, in situ X-ray photoelectron spectroscopy, and transmission electron microscopy. No intermediate ternary phases are formed and BiFeO3 crystallization is initiated in the Bi2 O3 layers at 450 °C following the diffusion-driven intermixing of the cations. Our study of the BiFeO3 formation provides an insight into the complex interplay between microstructural evolution, grain growth, and bismuth oxide evaporation, with implications for optimization of ferroelectric properties.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app