Synthesis and luminescence properties of Ba<sub>3</sub>Lu(PO<sub>4</sub>)<sub>3</sub>:Sm<sup>3+</sup> phosphor for white light-emitting diodes.

Optics Express 2017 April 18
A series of Ba<sub>3</sub>Lu(PO<sub>4</sub>)<sub>3</sub>:Sm<sup>3+</sup> phosphors were prepared by traditional high temperature solid-state reaction methods. The site-preferred occupancy of Sm<sup>3+</sup> in Ba<sub>3</sub>Lu(PO<sub>4</sub>)<sub>3</sub> and the luminescence properties of Ba<sub>3</sub>Lu(PO<sub>4</sub>)<sub>3</sub>:Sm<sup>3+</sup> were studied combined with X-ray diffraction, photoluminescence excitation (PLE) spectra, and emission (PL) spectra as well as temperature-dependent PL and decay curves. The PL intensity is improved with increasing Sm<sup>3+</sup> content and the optimal dopant content is 0.05. The temperature-dependent PL spectra indicate that the emission intensity decreases with the temperature because of the enhancement of the non-radiative transition. The results indicate that these reddish-orange emitting phosphors could be for potential applications in w-LEDs.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app