Chiral Metal-Oxide Nanofilms by Cellulose Template Using Atomic Layer Deposition Process.
ACS Nano 2017 May 24
In this article, we describe an advance approach for the fabrication of chiral metal-oxide nanofilms. Our approach is based on the atomic layer deposition of titania and alumina nanofilms onto cellulose microfibers, used as chiral templates, leading to the formation of chiral nanofilms with a spatial fibrous structure. The chiral nanofilms were extensively characterized by X-ray photoelectron spectroscopy and high-resolution electron microscopy. The chiral property of the produced titania nanofilms was studied by enantioselective adsorption experiments using circular-dichroism spectroscopy and chiral high-performance liquid chromatography. We demonstrate the application of the titania chiral nanofilms for enantioselective crystallization. Overall, the basic principle for the preparation of chiral nanofilms by atomic layer deposition is demonstrated, as well as their uses for several enantioselective applications.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app