Origin of a Nanoindentation Pop-in Event in Silicon Crystal.
Physical Review Letters 2017 March 4
The Letter concerns surface nanodeformation of Si crystal using atomistic simulation. Our results account for both the occurrence and absence of pop-in events during nanoindentation. We have identified two distinct processes responsible for indentation deformation based on load-depth response, stress-induced evolution of crystalline structure and surface profile. The first, resulting in a pop-in, consists of the extrusion of the crystalline high pressure Si-III/XII phase, while the second, without a pop-in, relies on a flow of amorphized Si to the crystal surface. Of particular interest to silicon technology will be our clarification of the interplay among amorphization, crystal-to-crystal transition, and extrusion of transformed material to the surface.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app