Corrosion Protection of Copper Using Al 2 O 3 , TiO 2 , ZnO, HfO 2 , and ZrO 2 Atomic Layer Deposition.
ACS Applied Materials & Interfaces 2017 Februrary 2
Atomic layer deposition (ALD) is a viable means to add corrosion protection to copper metal. Ultrathin films of Al2 O3 , TiO2 , ZnO, HfO2 , and ZrO2 were deposited on copper metal using ALD, and their corrosion protection properties were measured using electrochemical impedance spectroscopy (EIS) and linear sweep voltammetry (LSV). Analysis of ∼50 nm thick films of each metal oxide demonstrated low electrochemical porosity and provided enhanced corrosion protection from aqueous NaCl solution. The surface pretreatment and roughness was found to affect the extent of the corrosion protection. Films of Al2 O3 or HfO2 provided the highest level of initial corrosion protection, but films of HfO2 exhibited the best coating quality after extended exposure. This is the first reported instance of using ultrathin films of HfO2 or ZrO2 produced with ALD for corrosion protection, and both are promising materials for corrosion protection.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app