Ultra fast ultrasound-assisted decopperization from copper anode slime.

An ultra fast decopperization method from the anode slime has been developed based on the ultrasound-assisted leaching. The effects of parameters such as ultrasound power, leaching time, sulfuric acid concentration and liquid/solid ratio were investigated. Under optimum conditions, the concentration of Cu in residue was only 2.64%. The removal efficiency increases considerably and the decopperization time was significantly shortened comparing with conventional method (>10%, 24h). Se and Te have not been detected in lixivium, indicating the selective leaching of Cu. In addition, the mineralogical characteristics of the untreated anode slime and the residues after ultrasound-assisted decopperization are investigated. The results revealed that the increasing of decopperization efficiency was attributed to the change of the phase composition and the morphology and size of samples during ultrasound-assisted decopperization.

Full text links

We have located links that may give you full text access.
Can't access the paper?
Try logging in through your university/institutional subscription. For a smoother one-click institutional access experience, please use our mobile app.

Related Resources

For the best experience, use the Read mobile app

Mobile app image

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app

All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.

By using this service, you agree to our terms of use and privacy policy.

Your Privacy Choices Toggle icon

You can now claim free CME credits for this literature searchClaim now

Get seemless 1-tap access through your institution/university

For the best experience, use the Read mobile app