Clinical Study
Journal Article
Color changes of esthetic orthodontic ligatures evaluated by orthodontists and patients: a clinical study.
Dental Press Journal of Orthodontics 2016 September
Objective:: To evaluate in vivo changes in the color of esthetic elastomeric ligatures from different manufacturers.
Methods:: Four widely used commercial brands of elastomeric ligatures were selected and used in 20 adult patients in a split-mouth design. The ligatures were evaluated by orthodontists and patients in a double-blind manner on the day the ligatures were placed (T0) and 30 days after intraoral exposure (T1) by means of a system of staining scores. Groups were compared by Friedman test with p < 0.05.
Results:: Orthodontists and patients reported similar staining scores (p > 0.05). Results showed that all brands underwent significant staining when exposed to the intraoral environment. Modular-crystal MorelliTM (Sorocaba, SP, Brazil) showed the highest degree of staining with the median reaching the maximum value (3); while the other brands (3M UnitekTM, American OrthodonticsTM and GAC DentsplyTM) showed the median equal to 1 (p < 0.001). A large individual variability in the degree of staining was also found for all brands.
Conclusions:: All four brands of esthetic ligatures showed significant staining, which appeared to be more pronounced for the MorelliTM brand. Changes in color of the elastomeric ligatures were perceived similarly by patients and orthodontists. The industry needs to improve the color stability of esthetic ligatures.
Methods:: Four widely used commercial brands of elastomeric ligatures were selected and used in 20 adult patients in a split-mouth design. The ligatures were evaluated by orthodontists and patients in a double-blind manner on the day the ligatures were placed (T0) and 30 days after intraoral exposure (T1) by means of a system of staining scores. Groups were compared by Friedman test with p < 0.05.
Results:: Orthodontists and patients reported similar staining scores (p > 0.05). Results showed that all brands underwent significant staining when exposed to the intraoral environment. Modular-crystal MorelliTM (Sorocaba, SP, Brazil) showed the highest degree of staining with the median reaching the maximum value (3); while the other brands (3M UnitekTM, American OrthodonticsTM and GAC DentsplyTM) showed the median equal to 1 (p < 0.001). A large individual variability in the degree of staining was also found for all brands.
Conclusions:: All four brands of esthetic ligatures showed significant staining, which appeared to be more pronounced for the MorelliTM brand. Changes in color of the elastomeric ligatures were perceived similarly by patients and orthodontists. The industry needs to improve the color stability of esthetic ligatures.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app