Nanoindentation of Carbon Nanostructures.
In the present research paper carbon nanostructures viz. single walled carbon nanotubes, multi-walled carbon nanotubes, single walled carbon nanohorns and graphene nanoplatelets have been synthesized by CVD technique, hydrothermal method, DC arc discharge method in liquid nitrogen and microwave technique respectively. After synthesis 5 mm thick pallets of given nanomaterial are prepared by making a paste in isopropyl alcohol and using polyvinylidene difluoride as a binder and then these pallets were used for nanoindentation measurements. Hardness, reduced modulus, stiffness, contact height and contact area have been measured using nanoindenter.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app