The effect of washing water temperature on resin-dentin micro-shear bond strength.
Dental Research Journal 2016 March
BACKGROUND: The purpose of this study was to evaluate the effect of washing water temperature on the micro-shear bond strength (μSBS) of composite resin to dentin using a two-step etch-and-rinse system and a two-step self-etching system.
MATERIALS AND METHODS: In this in vitro study, the intact dentins of buccal and lingual surfaces of healthy third molars were exposed. Dentin surfaces were rinsed with different temperatures of distilled water (20 s) before applying Single Bond (SB) or Clearfil SE Bond(SE). After applying the adhesive, composite cylinders (0.8 mm diameter and 1 mm length) were bonded to the teeth surfaces. After storing the specimens in 37°C distilled water for 48 h and thermocycling, μSBS test was done. Data were analyzed using analysis of variance, post hoc Tukey tests, paired samples t-test, and Fisher exact test (α = 0.05).
RESULTS: Temperature and interaction of temperature and type of bonding agent affected the bond strength. The bond strength of SB groups was significantly higher at 50°C washing than 5°C (P = 0.003) and 22°C (P = 0.019), but no significant difference was observed between SE groups. The bond strength of SE was significantly higher at 22°C than that of SB (P = 0.031), whereas the bond strength of SB was significantly higher at 50°C than that of SE (P = 0.007).
CONCLUSION: The use of high-temperature washing water is an appropriate method to enhance bond strength in etch-and-rinse systems.
MATERIALS AND METHODS: In this in vitro study, the intact dentins of buccal and lingual surfaces of healthy third molars were exposed. Dentin surfaces were rinsed with different temperatures of distilled water (20 s) before applying Single Bond (SB) or Clearfil SE Bond(SE). After applying the adhesive, composite cylinders (0.8 mm diameter and 1 mm length) were bonded to the teeth surfaces. After storing the specimens in 37°C distilled water for 48 h and thermocycling, μSBS test was done. Data were analyzed using analysis of variance, post hoc Tukey tests, paired samples t-test, and Fisher exact test (α = 0.05).
RESULTS: Temperature and interaction of temperature and type of bonding agent affected the bond strength. The bond strength of SB groups was significantly higher at 50°C washing than 5°C (P = 0.003) and 22°C (P = 0.019), but no significant difference was observed between SE groups. The bond strength of SE was significantly higher at 22°C than that of SB (P = 0.031), whereas the bond strength of SB was significantly higher at 50°C than that of SE (P = 0.007).
CONCLUSION: The use of high-temperature washing water is an appropriate method to enhance bond strength in etch-and-rinse systems.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app