Surface analysis of pilot distribution system pipe autopsies: The relationship of organic and inorganic deposits to input water quality.
Water Research 2015 December 16
Time-of-Flight Secondary Ion Mass Spectrometry (ToF-SIMS) surface analysis was conducted to characterise deposits in polyethylene pipes used in a novel pilot water distribution system (PDS). The system consisted of four (4) parallel distribution systems receiving water from different treatment processes, ranging from conventional coagulation through to an advanced membrane filtration system. After two years of operation, the distribution system was shut down and samples of pipe were collected for autopsy analysis. Inlet and outlet samples from each PDS were collected for purpose of comparison. ToF-SIMS was used to assess chemical differences in surface biofilm accumulation and particulate deposition, which resulted as a consequence of the treatment method and operational mode of each system. These data supplemented previously collected bacteriological and chemical water quality data. Results from the inorganic analysis of the pipes were consistent with corrosion and contamination events that occurred upstream in the corresponding treatment systems. Principal component analysis of data on organic constituents showed oxygen and nitrogen containing fragments were associated with the treatment inlet and outlet samples. These types of signals can often be ascribed to biofilm polysaccharides and proteins. A trend was observed when comparing samples from the same PDS, showing an association of lower molecular weight (MW) organic fragments with the inlet and higher MW organic fragments with the outlet samples.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app