Impact strength of denture base and reline acrylic resins: An in vitro study.
This study evaluated the impact strength of a denture base resin (Lucitone 550-L) and four reline resins (Tokuyama Rebase II-T; Ufi Gel Hard-U; New Truliner-NT, and Kooliner-K), both intact and in a reline combination (L/L, L/T, L/U, L/NT, and L/K). For each group (n = 20), half of the specimens were thermocycled before testing. Charpy tests were performed, and the impact strengths were calculated. Data were analyzed by two-way analyses of variance and Tukey's test (p = 0.05). For the intact groups, mean impact strength values for L (1.65 and 1.50) were significantly higher than those of the reline resins (0.38-1.17). For the relined groups, the highest mean impact strength values were produced by L/T (5.76 and 5.12), L/NT (6.20 and 6.03), and L/K (5.60 and 5.31) and the lowest by L/U (0.76 and 0.78). There were no significant differences between L and L/L. Thermocycling reduced the impact strength of T (from 0.73 to 0.38) and L/L (from 1.82 to 1.56).
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app