Impact of galvanic corrosion on lead release from aged lead service lines.
Water Research 2012 October 16
Partial lead service line replacement (PLSLR) may be performed when tap water lead concentrations exceed the action level and in association with water main replacement or other maintenance. Partially replacing lead pipes with copper tubing can create a galvanic couple if the lead and copper are connected by a metal coupling, which can potentially enhance lead release by galvanic corrosion. The effect of two types of couplings, brass and plastic, on lead release after a simulated PLSLR was investigated in a set of laboratory-scale experiments. Experiments were conducted in a recirculation flow mode with intermittent stagnation periods using aged lead pipes harvested from Providence, RI. Release of both dissolved and particulate lead was higher for the brass-coupled systems than for the plastic-coupled systems, and galvanic corrosion was the primary cause of significant particulate lead release from the brass-coupled systems. For brass-coupled systems, longer stagnation times resulted in dramatically more release of particulate lead. Sampling of different volumes following stagnation showed that lead release for the brass-coupled systems was locally much higher in the region closest to the coupling. The impact of galvanic corrosion persisted for the six weeks of the experiment.
Full text links
Related Resources
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app
All material on this website is protected by copyright, Copyright © 1994-2024 by WebMD LLC.
This website also contains material copyrighted by 3rd parties.
By using this service, you agree to our terms of use and privacy policy.
Your Privacy Choices
You can now claim free CME credits for this literature searchClaim now
Get seemless 1-tap access through your institution/university
For the best experience, use the Read mobile app